133426. Custom Hastelloy C22 Wire Supplier Short Lead Time with ASTM B574 Standard
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133427. Hastelloy C276 Cold-Drawn Wire Excellent Dimensional Accuracy Smooth Surface for Spring Coiling
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133428. Precision Drawn Hastelloy C276 C22 B2 Wire, Custom Diameter for Springs Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133429. Precision Drawn Hastelloy C276 C22 B2 Wire, Custom Diameter for Springs Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133430. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133431. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133432. Spring Temper Hastelloy C276 C22 Wire High Tensile Strength for Precision Fasteners
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133433. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133434. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133435. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133436. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133437. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133438. Hastelloy C22 C276 C4 B2 Wire for Petrochemical Furnace Components Oxidation Resistance
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133439. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...
133440. Hastelloy C276 C22 Coil Spool Wire for Chemical Processing Crevice Corrosion Chloride
[Jul 27, 2026]
[Jul 27, 2026] Product Description Grades Density (g/cm³) Melting Point (°C) C-276 8.9 1325-1370 °C C-22 8.69 1325-1370 °C C-4 8.64 1350-1380°C B-2 9.2 1350-1380°C B-3 9.2 1370-1418°C Features * Provides excellent resistance to both ...