751. Fast-Flash Rust Inhibitive Water-Based Coating
[Aug 25, 2026]
[Aug 25, 2026] Detailed Photos Product Description This product is a one-component acrylic amino paint suitable for iron, electrophoresis and other substrates. It is made of water-soluble acrylic resin, amino resin, additives, ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
752. Low-Voc Hammer Tone Coating (VOC<150g/L) for Eco-Certified Factories
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
753. Acid Rain Resistant Water-Based Coating for Urban Infrastructure
[Aug 25, 2026]
[Aug 25, 2026] Detailed Photos Product Description This product is a one-component acrylic amino paint suitable for iron, electrophoresis and other substrates. It is made of water-soluble acrylic resin, amino resin, additives, ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
754. Vinyl-Toluenated Alkyd Coating for Chemical Resistance
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
755. Self-Repairing Water-Based Coating for Ship Hulls
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
756. Fast-Drying Water-Based Anti-Corrosion Coating for DIY Projects
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
757. Quick-Cure UV Glass Coating for High-Speed Production
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
758. Flexible Glass Coating for Tempered Glass Surfaces
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
759. Static-Dissipative Coating for Electronics Factories
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
760. Aerogel-Enhanced Thermal Barrier Polyurethane Coating
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
761. Temperature-Adaptive Rust Prevention Coating (± 50° C)
[Aug 25, 2026]
[Aug 25, 2026] Detailed Photos Product Description This product is a one-component acrylic amino paint suitable for iron, electrophoresis and other substrates. It is made of water-soluble acrylic resin, amino resin, additives, ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
762. Quick-Dry Alkyd Coating for Maintenance and Repair Projects
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
763. Water-Reducible Alkyd Coating for Environmental Compliance
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
764. Mold-Resistant Alkyd Coating for Humid Environments
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.
765. Advanced Water Based Anti Rust Coating for Humid Climate Protection Metal
[Aug 25, 2026]
[Aug 25, 2026] Coating process requirements 1. The coating operation should be carried out under the environmental conditions of 5~35ºC and relative humidity below 80%, and the surface temperature of the substrate should be ...
Company: Jiangsu Shuocheng New Materials Technology Co., Ltd.